Anodization

Formation of hard aluminum oxide surface by electrolysis  
last edit 2005 10 28

Cleaning.

Wash the aluminum part very  carefully with soap.  Make shure all  fat, oil dirt and fingerprints are removed. Use gloves. Rince in  fresh water. Dip the part in  sodium hydroxide solution (NaOH). Appr 1-3g per 300 ml water. Let soda  react with the aluminum surace for appr 10 minutes. Hydrogen gas will build up. Ventilate. The surface should be grey and  matt after the soda treatment.

The cleaning of the aluminum part is very important.

Rince directly with resh water. Never touch the surface.

Electrolysis

Doppa ner i elektrolysbadet ca 20% svavelsyra.  Pluspol till objekt, minuspol till aluminium elektrod.
Var noggran med att få elektrisk kontakt, spänn fast objektet noggrant, gärna med en gängad skruv eller ett vasst stift som pressas mot ytan. Obs Allt måste vara i aluminium.

Ca 2-3 Ampere i 1-2 timmar för en liten pryl typ hylsa 4 cm lång 3cm  ca  i diameter.

Obs vätskan blir varm efter ett tag så kylning är bra. Typ stå i en yttre kall bytta eller slangar med kallvatten.Utsug. Det stinker svavelsyrapartiklar efter ett tag. Ju kallare elektrolysbad  desto bättre hårdare yta. Gärna ner till iskallt(4grader C)  om möjligt. Skölj i vatten.
Doppa ner i färgämnet. I detta fall  blått bläck utspädd med 4 delar vatten.

Låt ligga i ett par timmar.

 

Många färgämnen funkar bättre eller sämre, inget färgämne ger dock helt svart yta, då måste man köpa special färgämnen (nigrocin tex),  blått bläck ger dock en fin blå lyster. Man får laborera sig fram till ett bra infärgning.

Rince 

Lägg i en kastrull med vatten och härda med kokande vatten ca 15-30min.


A fine blue color and a hard surface